  • Current Research in Dental Sciences
  • Volume:26 Issue:3
  • İKİ FARKLI DİŞ MACUNUNUN FARKLI RESTORATİF MATERYALLERİN YÜZEY PÜRÜZLÜLÜĞÜ ÜZERİNE ETKİSİ...

İKİ FARKLI DİŞ MACUNUNUN FARKLI RESTORATİF MATERYALLERİN YÜZEY PÜRÜZLÜLÜĞÜ ÜZERİNE ETKİSİ

Authors : Kanşad PALA, Neslihan TEKÇE, Hale KARAKUYU, Emre ÖZEL
Pages : 399-406
Doi:10.17567/ataunidfd.290243
View : 19 | Download : 18
Publication Date : 2016-12-01
Article Type : Research Paper
Abstract :Amaç : Bu çalışmanın amacı, diş macunlarının farklı restoratif materyallerin yüzey pürüzlülüğüne etkisini incelemektir. Gereç ve Yöntem :Bu çalışmada toplam 40 adet kom- pozit disk oluşturulmuştur. Kompozit diskler iki direkt kompozit [Aelite All Purpose Body insert ignore into journalissuearticles values(Bisco, Schaumburg, IL, Amerika);, Clearfil Majesty Posterior, insert ignore into journalissuearticles values(Kuraray Medi- cal Inc, Tokyo, Japonya);], bir indirekt [Epricord insert ignore into journalissuearticles values(Ku- raray);] kompozit ve bir kompomer [insert ignore into journalissuearticles values(Dyract XP insert ignore into journalissuearticles values(Dyract XP, D entsply , Konstanz, Almanya);] materyallerinden oluşturulmuştur insert ignore into journalissuearticles values(n=10);. Hazırlanan kompozitlerin cila- ları PoGo kitleri ile yapılmıştır. Her bir grupta yer alan kompozitler ikiye ayrılmış insert ignore into journalissuearticles values(n=5); ve bu alt gruplara iki farklı diş macunu insert ignore into journalissuearticles values(Colgate, Sensodyne); bir elektrikli diş fırçası aracılığıyla 12 dakika boyunca uygulanmıştır. Her bir örneğin başlangıç, cila sonrası ve diş fırçalama sonrası değerleri ayrı ayrı kaydedilmiştir. İstatistiksel analizler repeated tek yönlü varyans analizi insert ignore into journalissuearticles values(Anova); ile yapılmıştır insert ignore into journalissuearticles values(p<0.05);. Bulgular :Bütün gruplarda en düşük pürüzlülük değer- lerini anlamlı olarak şeffaf bant altında hazırlanan ör- nekler sergilemiştir insert ignore into journalissuearticles values(p < 0.05);. Polisajdan sonra en dü- şük pürüzlülük değerini Aelite insert ignore into journalissuearticles values(0,347±0,21);, en yüksek pürüzlülük değerlerini Dyract XP insert ignore into journalissuearticles values(0,453±0,11); sergile- miştir insert ignore into journalissuearticles values(p > 0.05);. Sonuç : Bu çalışmada kullanılan bütün restoratif ma- teryaller iki farklı diş macunu ile fırçalanma işlemi ar- kasından istatistiksel olarak başlangıç değerleri ile ben- zer sonuçlar sergilemiştir. Ancak Sensodyne; Aelite, Majesty Posterior ve Dyract XP’nin pürüzsüzlüğünü hafif düzeyde geliştirirken, Colgate Epricord ve Dyract XP’nin pürüzsüzlüğünü hafif düzeyde geliştirmiştir. Anahtar Kelimeler : Rezin kompozit, mikrohibrit, nanohibrit, diş macunu, yüzey pürüzlülüğü EFFECT OF THE TWO DİFFERENT TOOTHPASTES ON SURFACE ROUGHNESS  OF DIFFERENT RESTORATIVE MATERIALS Aim: The aim of this study was to investigate the effect of toothpastes on surface roughness ​​of different restorative materials. Materials and Methods: 40 composite discs were created for this study. Composite disc are constituted from two direct composites [Aelite All Purpose Body insert ignore into journalissuearticles values(Bisco, Schaumburg, IL, USA);, Clearfil Majesty Posterior, insert ignore into journalissuearticles values(Kuraray Medical Inc, Tokyo, Japan);], an indirect composite [Epricord insert ignore into journalissuearticles values(Kuraray);] and a compomer [insert ignore into journalissuearticles values(Dyract XP insert ignore into journalissuearticles values(Dyract XP, D entsply , Germany);] insert ignore into journalissuearticles values(n=10);. The PoGo kit was used for finishing and polishing procedures. Each composite group were divided into two insert ignore into journalissuearticles values(n=5); and two different toothpaste insert ignore into journalissuearticles values(Colgate, Sensodyne); were applied by an electric toothbrush for 12 minutes. Initial values, and after polishing and tooth brushing values for each material were recorded separately. Statistical analysis was performed by one-way ANOVA insert ignore into journalissuearticles values(p<0.05);. Results: In all groups; the lowest roughness values were obtained from examples prepared under the mylar strip insert ignore into journalissuearticles values(significantly); insert ignore into journalissuearticles values(p < 0.05 );. After polishing, Aelite insert ignore into journalissuearticles values(0.347±0.21); exhibited the lowest roughness values, and Dyract XP insert ignore into journalissuearticles values(0.453±0.11); exhibited the highest values insert ignore into journalissuearticles values(p > 0.05);. Conclusion: All restorative materials used in this study exhibited statistically similar results after tooth brushing with two different toothpastes according to baseline. Sensodyne improved smoothness of Aelite, Majesty Posterior and Dyract XP, while Colgate improved smoothness of Epricord and Dyract XP. Keywords: Resin composite, microhybrid, nanohybrid, toothpaste, surface roughness
Keywords : Rezin kompozit, mikrohibrit, nanohibrit, diş macunu

ORIGINAL ARTICLE URL
VIEW PAPER (PDF)

* There may have been changes in the journal, article,conference, book, preprint etc. informations. Therefore, it would be appropriate to follow the information on the official page of the source. The information here is shared for informational purposes. IAD is not responsible for incorrect or missing information.


Index of Academic Documents
İzmir Academy Association
CopyRight © 2023-2025