  • PROFİLAKTİK PAT VE BEYAZLATMA UYGULAMASININ FARKLI KOMPOZİT REZİNLERİN MİKROSERTLİKLERİ ÜZERİNE ETKİ...

PROFİLAKTİK PAT VE BEYAZLATMA UYGULAMASININ FARKLI KOMPOZİT REZİNLERİN MİKROSERTLİKLERİ ÜZERİNE ETKİSİ

Authors : Fatma Dilşad ÖZ, Ceren Özge BİÇER, Nuray ATTAR, Yonca KORKMAZ
Pages : 285-291
Doi:10.17567/ataunidfd.416928
View : 24 | Download : 7
Publication Date : 2018-07-11
Article Type : Research Paper
Abstract :Amaç: Bu çalışmanın amacı, profilaktik pat ve beyazlatma uygulamalarının ardından farklı tip kompozitlerin mikrosertliklerini değerlendirmektir. Gereç ve Yöntem: Şeffaf bant ile kapatılmış cam kalıplarda, nanohibrid insert ignore into journalissuearticles values(GrandioSO); insert ignore into journalissuearticles values(Grup A); , nanodolduruculu akışkan insert ignore into journalissuearticles values(Filtek Supreme XT Flow); insert ignore into journalissuearticles values(Grup B); ve nanodolduruculu kompozit insert ignore into journalissuearticles values(Filtek Ultimate); insert ignore into journalissuearticles values(Grup C); ile toplam 120 örnek insert ignore into journalissuearticles values(her bir restoratif materyal için 40 örnek); hazırlanmıştır. Polimerizasyonun ardından tüm örneklere Sof-Lex Disk Sistemi ile bitirme ve polisaj işlemleri uygulanmış ve her bir restoratif materyalin örnekleri 4 gruba ayrılmıştır. Grup 1: 37°C distile suda iki hafta bekletilmiştir insert ignore into journalissuearticles values(kontrol);, Grup 2: Proxyt Fine profilaktik pat uygulanmıştır, Grup 3: Pola Office insert ignore into journalissuearticles values(SDI + beyazlatma yapılmıştır, Grup 4: Proxyt Fine profilaktik pat uygulaması + Pola Office+ beyazlatma yapılmıştır insert ignore into journalissuearticles values(toplam 12 grup);. Mikrosertlik ölçümleri dijital bir mikrosertlik test cihazı ile gerçekleştirilmiştir insert ignore into journalissuearticles values(HMV-2, SHIMADZU , Kyoto, Japonya);   insert ignore into journalissuearticles values(yük 500 g; bekleme süresi 15 saniye);. Veriler tek yönlü ANOVA test ile analiz edilmiştir. Çoklu karşılaştırmalar Tukey test ile gerçekleştirilmiştir insert ignore into journalissuearticles values( p<0.05 );. Bulgular: GrandioSO materyali için insert ignore into journalissuearticles values(A);, Grup A4, Grup A1’den istatistiksel olarak anlamlı derecede daha düşük mikrosertlik değerleri göstermiştir insert ignore into journalissuearticles values(p<0.001); ancak Grup A1, A2 ve A3 arasında fark yoktur insert ignore into journalissuearticles values(p=0.51);.   Filtek Supreme XT Flow insert ignore into journalissuearticles values(B); için 4 grup arasında istatistiksel olarak fark yoktur insert ignore into journalissuearticles values(p=0.24);. Filtek Ultimate materyali için insert ignore into journalissuearticles values(C);, Grup C1 ve C2, Grup C3 ve C4’ten istatistiksel olarak anlamlı derecede daha yüksek mikrosertlik değerleri göstermiştir insert ignore into journalissuearticles values( p<0.01 );. Tüm gruplar için, Filtek Supreme XT Flow insert ignore into journalissuearticles values(B); GrandioSO insert ignore into journalissuearticles values(A); ve Filtek Ultimate insert ignore into journalissuearticles values(C); gruplarından anlamlı derecede daha düşük mikrosertlik değerleri göstermiştir insert ignore into journalissuearticles values( p<0.01 );. Sonuç: Profilaktik pat ve beyazlatmanın birlikte uygulanması ya da tek başına beyazlatma işlemi kompozitlerin mikrosertliğini materyalin türüne bağlı olarak olumsuz etkileyebilir. Anahtar Kelimeler: Kompozit rezinler, diş beyazlatma, diş parlatma The Influence of Prophylactic Paste and Bleaching on the Microhardness of Different Composite Resins Abstract Objective: The aim of this study was to evaluate the microhardness of different types of composites after application of prophylactic paste and bleaching. Materials and Methods: A total of 120 specimens insert ignore into journalissuearticles values(40 specimens for each restorative materials); were fabricated using a nanohybrid insert ignore into journalissuearticles values(GrandioSO ); insert ignore into journalissuearticles values(Group A);, a nanofill flowable insert ignore into journalissuearticles values(Filtek Supreme XT Flow); insert ignore into journalissuearticles values(Group B); and a nanofill composite resin insert ignore into journalissuearticles values(Filtek Ultimate); insert ignore into journalissuearticles values(Group C); in a plexiglass mold covered with a Mylar strip. After polymerization, all specimens were finished and polished with Sof-Lex insert ignore into journalissuearticles values(3M ESPE); Polishing disc   system and each restorative material specimens were divided into four treatment groups: Group 1: stored in distilled water at 37°C for two weeks insert ignore into journalissuearticles values(control);, Group 2: Application of Proxyt Fine   Prophylactic paste, Group 3: Bleaching with Pola Office + and Group 4: Application of Proxyt Fine Prophylactic paste + bleaching with Pola Office+ insert ignore into journalissuearticles values(totally 12 groups);. The microhardness measurements were performed using a digital microhardness tester insert ignore into journalissuearticles values(HMV-2, SHIMADZU , Kyoto, Japan);   insert ignore into journalissuearticles values(load 500 g; dwell time 15 seconds);. The data were analyzed using the one-way ANOVA test. Multiple comparison was performed with the Tukey HSD test insert ignore into journalissuearticles values(p<0.05);. Results: For GrandioSO insert ignore into journalissuearticles values(A);, Group A4 exhibited statistically significant lower microhardness values than Group A1 insert ignore into journalissuearticles values(p<0.001); but there were no difference among Groups A1, A2 and A3 insert ignore into journalissuearticles values(p=0.51);.   In Filtek Supreme XT Flow insert ignore into journalissuearticles values(B); there were no statistically significant difference for all 4 groups insert ignore into journalissuearticles values(p=0.24);. In terms of Filtek Ultimate insert ignore into journalissuearticles values(C);, Group C1 and C2 showed statistically significant higher microhardness values than Group C3 and C4 insert ignore into journalissuearticles values(p<0.01);. For all main groups, Filtek Supreme XT Flow insert ignore into journalissuearticles values(B); exhibited statistically significant lower microhardness values than   GrandioSO insert ignore into journalissuearticles values(A); and Filtek Ultimateinsert ignore into journalissuearticles values(C); insert ignore into journalissuearticles values(p<0.01);. Conclusion: Application of Prophylactic Paste and bleaching procedure together or bleaching procedure alone may negatively affect the microhardness of composites depending on the type. Key Words: Composite resins, tooth bleaching, dental polishing
Keywords : Kompozit rezinler, diş beyazlatma

ORIGINAL ARTICLE URL
VIEW PAPER (PDF)

* There may have been changes in the journal, article,conference, book, preprint etc. informations. Therefore, it would be appropriate to follow the information on the official page of the source. The information here is shared for informational purposes. IAD is not responsible for incorrect or missing information.


Index of Academic Documents
İzmir Academy Association
CopyRight © 2023-2025