  • Effects of Three Aging Methods on Colour Differences of All-Ceramic Materials

Effects of Three Aging Methods on Colour Differences of All-Ceramic Materials

Authors : Tugba TEMIZCI, Ali Rıza TUNÇDEMİR
Pages : 1-17
View : 46 | Download : 7
Publication Date : 2020-12-29
Article Type : Research Paper
Abstract :Objective. The aim of the study is to test the effects of three different aging methods on colour change (E00) in three different all-ceramic systems prepared in two thicknesses (0.5 and 1.0 mm). Materials and methods. Zirconia Katana UTML (ZK), Prettau Anterior (PA) and IPS-e.max press (EP) prepared in two thicknesses were tested using in vitro artificial accelerated aging (AAA), thermocycling (TC) and autoclave aging (AA) methods. The effects on the colour (CIE L*a*b*) differences were determined using a spectrophotometer and evaluated by analysis of variance (ANOVA). Results. The aging protocols affected the E00-values of the ceramic systems at different levels (0.64–2.69), and the ceramic thicknesses were statistically significant (P <0.5). Generally (excluding the 0.5-mm EP group), the highest E00 value among the methods of aging was in the AAA applied samples, followed by those in the TC and the AA. Also, the ceramic thickness was found to be significant in testing aging protocols. In addition, the E00-values of the ceramic materials tested were below the clinically accepted level. Conclusions. Three ceramic types – prepared in two different thicknesses and applied for three 1-year in vitro aging protocols – were affected at different levels by the aging methods tested, and significant colour differences were determined among all the ceramic samples. Clinical Significance: One-year applications of three aging protocols (AAA, TC and AA) resulted in significant differences in the E00-values of ceramic systems (ZK, PA and EP). The differences between the E00-values among the aging tests in the all-ceramic types and the all-ceramic thicknesses were significant.
Keywords : Accelerated aging, Autoclave aging, Thermocycling, Colour stability, Dental ceramics

ORIGINAL ARTICLE URL

* There may have been changes in the journal, article,conference, book, preprint etc. informations. Therefore, it would be appropriate to follow the information on the official page of the source. The information here is shared for informational purposes. IAD is not responsible for incorrect or missing information.