IAD Index of Academic Documents
  • Home Page
  • About
    • About Izmir Academy Association
    • About IAD Index
    • IAD Team
    • IAD Logos and Links
    • Policies
    • Contact
  • Submit A Journal
  • Submit A Conference
  • Submit Paper/Book
    • Submit a Preprint
    • Submit a Book
  • Contact
  • European Journal of Research in Dentistry
  • Volume:1 Issue:1
  • A Comparative Study of Shear Bond Strength of Three Different Bracket Bases Bonded to Porcelain Surf...

A Comparative Study of Shear Bond Strength of Three Different Bracket Bases Bonded to Porcelain Surfaces

Authors : Göksu TRAKYALI, Gülden SINMAZIŞIK
Pages : 24-28
Doi:10.12990/MDJ2013124
View : 24 | Download : 10
Publication Date : 2013-07-29
Article Type : Research Paper
Abstract :Previous studies showed that the bonding strength of brackets to porcelain restorations and the failure model depend on many variables including bracket base design. The aim of this in-vitro study was to investigate Shear Bond Strength insert ignore into journalissuearticles values(SBS); of different bracket base designs on porcelain surfaces and to evaluate the sites of adhesive fracture with the Adhesive Remnant Index insert ignore into journalissuearticles values(ARI);. Sixty feldspathic porcelain discs were randomly divided into three different groups each of twenty. Maxillary right incisor metal brackets with three different base designs insert ignore into journalissuearticles values(Victory series, 3M Unitek, Monrovia, California; Dyna-Lock, 3M Unitek, Monrovia, California and Mini Topic, Dentaurum, Inspringen, Germany); were bonded on the deglazed and conditioned porcelain surfaces in group 1, 2 and 3 respectively. Brackets were debonded and SBS was calculated in Mega Pascal insert ignore into journalissuearticles values(MPa);. ARI scores were recorded after debonding. SBS forces calculated for group 1, 2 and 3 were 20,57 insert ignore into journalissuearticles values(± 7,18);, 16,84 insert ignore into journalissuearticles values(± 6,20);, 18,55 insert ignore into journalissuearticles values(± 5,46); MPa respectively. ANOVA and Multiple Comparison test revealed no significant difference in ARI scores between groups. Porcelain fractures after debonding were observed in groups 1 and 3. All brackets tested provided acceptable SBS. However, only Dyna-Lock brackets did not cause any porcelain fractures at debonding. This finding could be an acceptable reason to use this kind of brackets during orthodontic treatment of patient having porcelain restorations.
Keywords : Orthodontics, bracket base, dental porcelain, shear bond strength,

ORIGINAL ARTICLE URL
VIEW PAPER (PDF)

* There may have been changes in the journal, article,conference, book, preprint etc. informations. Therefore, it would be appropriate to follow the information on the official page of the source. The information here is shared for informational purposes. IAD is not responsible for incorrect or missing information.


Index of Academic Documents
İzmir Academy Association
CopyRight © 2023-2025